W-10Zn

  • W-10 is a tin bronze alloy also classified as red bronze or leaded gunmetal.
  • The W-10Zn is a hard water resistant material which is ideal for applications such as sliding bearings and coupling pieces submitted to moderate forces.
  • It’s available as a round bar, rectangular bar, square bar, half moon, H shape and also based on client’s designs.

 

Chemical composition
% min. % máx
Cu Resto
Sn  9 11
Pb 2,0
Zn 1,0 3,0
P 0,2
Fe 0,25
Ni1 2,0
Sb 0,3
S  0,1


1
Niquel cuenta como Cobre.

Mechanical properties (Minimum values)
Proceso de moldeo y designación Continuous (GC) Centrifugal (GZ)
Tensile Strength
Rm (MPa)
140 150
Yield Point 0,2%
Rp0,2 (MPa)
280 280
Elongation 5D
A (%)
8 5
 HB-10-1000 90 95
Physical properties
Density
kg/dm3
8,7
Specific Heat
j/g. k
0,370
Thermal Expansion
10-6 k
18,0
Thermal Conductivity
W/m. ºk
71
Electrical Conductivity
m / (Ohm.mm2)
8,5

Closest international standards

Area Standards Former Code Former denomination
Alemania DIN 17656 : 1973 CuSn10Zn 2.1087 Rg10
Australia AS 1565 : 1996 C92610A C92610A 88/ 10/ 2 Gunmetal 905C
China GB 1176 : 1987 CuSn10Zn2 10 – 2 Zinn Bronze
Dinamarca DS 3001 : 1978 Tinbronze 5456 Rodgods 5456 Tinbronze 5456
España UNE 37-103-2 : 1981 CuSn10Zn2 C-3220
Finlandia SFS 2208 : 1977 CuSn10Zn2
Finlandia SFS 2208 : 1977 CuSn10Zn2
Hungría MSZ 8579 : 1984 CuSn10Zn2 Vöt 10
ISO ISO 1338 : 1977 CuSn10Zn2
Italia UNI 7013-10 : 1979 CuSn10Zn2Ni2 G-BS ZN2 NI2
Italia UNI 7013-6 : 1972 CuSn10Zn2 Bronzo allo zinco 88/ 10 / 2
Japón JIS H 5111 : 1988 BC 3 Class 3
Polonia PN / H-87026 : 1991 CuSn10Zn2 B102
Portugal NS 16512 : 1977 CuSn10Zn2 Tinnbronse Stopelegering
Portugal NP 1212 : 1976 CuSn10Zn2
Reino Unido BS 1400 : 1985 CuSn10Zn2 G1 Gunmetal CuSn10Zn2, G1
Republica Checa CSN 423138 : 1980 CuSn10Zn2 423138
Rusia GOST 613 : 1979 BrO10Z2
Suecia SIS 145458 : 1977 CuSn10Zn2 5458 Tennbrons 5458
USA ASTM B 584 : 1998 C92600 C92600
USA ASTM B 022 : 1995 C90500 C90500

Optional thermal treatments available on clients’ request

Proceso Temperature Time Enfriamiento Time
Stabilised 400°C 1.5h En horno 4h
Cambio de fase 630°C 1.5h En horno 6h